Difference between revisions of "Spot Welder"
(8 intermediate revisions by 3 users not shown) | |||
Line 5: | Line 5: | ||
|Is used in domain= | |Is used in domain= | ||
|Has name={{PAGENAME}} | |Has name={{PAGENAME}} | ||
+ | |Has make=Miller | ||
+ | |Has model=LMSW-52 | ||
+ | |Has serial number=MJ328801N | ||
+ | |Has life expectancy= | ||
+ | |Has year of manufacture or purchase= | ||
+ | |Has replacement cost= | ||
|Has icon=File: Spot_welderIcon.png | |Has icon=File: Spot_welderIcon.png | ||
|Has icondesc=Reflow Oven Icon | |Has icondesc=Reflow Oven Icon | ||
Line 11: | Line 17: | ||
|Has description= | |Has description= | ||
|Has certification=https://georgefox.instructure.com/courses/1281 | |Has certification=https://georgefox.instructure.com/courses/1281 | ||
− | |||
− | |||
− | |||
|Has group=Circuit Board Design | |Has group=Circuit Board Design | ||
− | |Has ace= | + | |Has ace=Needed;Makerhub@georgefox.edu |
}} | }} | ||
[[{{#show: {{FULLPAGENAME}}|?Has icon|link=none}}|140px|left|top|{{#show: {{FULLPAGENAME}}|?Has icondesc}}]] | [[{{#show: {{FULLPAGENAME}}|?Has icon|link=none}}|140px|left|top|{{#show: {{FULLPAGENAME}}|?Has icondesc}}]] | ||
Line 56: | Line 59: | ||
====Terminology==== | ====Terminology==== | ||
− | * | + | *Electrode Tips – The copper ends of the tongs that make contact with the workpiece to deliver welding current. |
+ | *Arms / Handles – The insulated portions you hold; provide leverage to open/close the tongs. | ||
+ | *Jaws – The part of the tongs where the electrode tips are mounted; may pivot to adjust pressure. | ||
+ | *Adjustment Knob / Screw – Used to set electrode pressure for consistent welds. | ||
+ | *Cable / Conductor – Heavy cable connecting the tongs to the welder to carry welding current. | ||
+ | *Spring Mechanism – Internal spring that helps return the tongs to the open position when released. | ||
+ | *Insulation / Grip – Protective covering to prevent electric shock and allow safe handling. | ||
==Training== | ==Training== | ||
Line 77: | Line 86: | ||
==Certification== | ==Certification== | ||
+ | Complete the <strong>Welding Shop - {{PAGENAME}} Module</strong> at the link below to gain access to the {{PAGENAME}}. The Maker Hub Canvas course pertains to all facilities and equipment contained in the Maker Hub; simply complete the quizzes for the facilities/equipment you wish to use in the Maker Hub. Please email <span style="color:blue">makerhub@georgefox.edu</span> if you have any questions. | ||
− | [https://georgefox.instructure.com/ | + | [https://georgefox.instructure.com/enroll/R6RF69 Maker Hub Canvas Course] |
==Troubleshooting== | ==Troubleshooting== | ||
+ | |||
+ | *No weld or weak weld: | ||
+ | **Check electrode tips for wear, dirt, or oxidation; clean or replace as needed. | ||
+ | **Verify proper electrode pressure; adjust using the adjustment knob/screw. | ||
+ | **Ensure cables are securely connected and not damaged. | ||
+ | *Sparks at handles / arcing: | ||
+ | **Inspect insulation on handles and tongs; replace if cracked or damaged. | ||
+ | **Confirm all connections are tight and corrosion-free. | ||
+ | *Tongs won’t open/close smoothly: | ||
+ | **Check spring mechanism for damage or debris; clean and lubricate lightly if needed. | ||
+ | **Ensure pivot points are not seized or misaligned. | ||
+ | *Overheating tongs: | ||
+ | **Reduce duty cycle; allow tongs to cool between welds. | ||
+ | **Check for proper current settings and electrode contact. | ||
+ | *Uneven welds: | ||
+ | **Inspect electrode tips for uneven wear; dress or replace as needed. | ||
+ | **Confirm correct alignment of jaws and consistent pressure. | ||
==Maintenance== | ==Maintenance== | ||
Line 93: | Line 120: | ||
!Done By | !Done By | ||
|- | |- | ||
− | | | + | |N/A |
− | + | |N/A | |
− | + | |N/A | |
− | |||
− | |||
− | |||
− | | | ||
− | | | ||
− | |||
− | |||
− | |||
− |
Latest revision as of 12:48, 15 August 2025
Make: Miller
Model: LMSW-52
Serial Number: MJ328801N
Ace: Needed (Makerhub@georgefox.edu).
Location: Welding Shop
Safety First
- Wear gloves and welding helmet.
- Don't have bare skin exposed.
- Don't weld in wet gear or standing water.
- Welded material will be hot.
Description
Resistance spot welding is a process in which contacting metal surface points are joined by the heat obtained from resistance to electric current. The Miller LMSW-52 Air-Cooled Spot Welder is a lightweight unit that is portable, easy to operate and excellent for welding mild, galvanized or stainless sheet materials.
- LMSW-52 spot welder manual [1]
Here is an example of spot welding and some good basic information.
Documentation
Terminology
- Electrode Tips – The copper ends of the tongs that make contact with the workpiece to deliver welding current.
- Arms / Handles – The insulated portions you hold; provide leverage to open/close the tongs.
- Jaws – The part of the tongs where the electrode tips are mounted; may pivot to adjust pressure.
- Adjustment Knob / Screw – Used to set electrode pressure for consistent welds.
- Cable / Conductor – Heavy cable connecting the tongs to the welder to carry welding current.
- Spring Mechanism – Internal spring that helps return the tongs to the open position when released.
- Insulation / Grip – Protective covering to prevent electric shock and allow safe handling.
Training
Operation
Here are some general setup rules of thumb:
- The maximum weld capacity is 2 sheets of 16 gauge material.
Demonstration
For the demonstration you will need to perform a spot weld using two pieces of scrap material.
General Procedure
- Ensure the material being welded should be clear of any oil or dust
- Turn on the spot welder
- Place the material being welded between the clamps.
- Clamp down on the two pieces of material for approximately 2 seconds. The time required to weld may vary slightly depending on the material and thickness.
- Grab workpiece with a set of pliers, and open the clamp.
Certification
Complete the Welding Shop - Spot Welder Module at the link below to gain access to the Spot Welder. The Maker Hub Canvas course pertains to all facilities and equipment contained in the Maker Hub; simply complete the quizzes for the facilities/equipment you wish to use in the Maker Hub. Please email makerhub@georgefox.edu if you have any questions.
Troubleshooting
- No weld or weak weld:
- Check electrode tips for wear, dirt, or oxidation; clean or replace as needed.
- Verify proper electrode pressure; adjust using the adjustment knob/screw.
- Ensure cables are securely connected and not damaged.
- Sparks at handles / arcing:
- Inspect insulation on handles and tongs; replace if cracked or damaged.
- Confirm all connections are tight and corrosion-free.
- Tongs won’t open/close smoothly:
- Check spring mechanism for damage or debris; clean and lubricate lightly if needed.
- Ensure pivot points are not seized or misaligned.
- Overheating tongs:
- Reduce duty cycle; allow tongs to cool between welds.
- Check for proper current settings and electrode contact.
- Uneven welds:
- Inspect electrode tips for uneven wear; dress or replace as needed.
- Confirm correct alignment of jaws and consistent pressure.
Maintenance
General maintenance
The welding tips should be inspected and cleaned as needed.
Specific Maintenance Tasks
Maintenance Procedure | Frequency | Done By |
---|---|---|
N/A | N/A | N/A |